Failure Analysis (FA) Equipment

  

Setting up a failure analysis laboratory from scratch is not easy nor cheap.  It goes without saying that the process of setting up an FA lab requires diligent planning up-front.  The two major aspects of setting up an FA lab are the preparation of the facility and the purchase of the FA equipment

            

Much thought needs to go into the correct choice of the FA equipment, since a lot of these are quite expensive.  Most companies set up their FA lab in stages, gradually building up the FA capability of the lab over time.  Many FA managers follow three (3) stages (Basic, Good, and Advanced capabilities) in setting up their FA labs, which are presented in Tables 1 to 3 below.

     

Table 1. Basic FA Capability

FA Equipment

Purpose

Estimated Cost (USD)

Curve Tracer and Break-out Boxes

I/V Curve Tracing

10K - 20K

Digital Multimeters

Bench Testing

5K - 10K

Power Supplies/Signal Generators

Bench Testing

5K - 10K

Oscilloscope

Bench Testing

10K - 20K

Low-power Microscope

Optical Inspection

5K - 10K

High-power Microscope

Optical Inspection

10K - 50K

Fume Hood and Glassware

Manual Decapsulation

5K - 15K

Vise and Assorted Hand Tools

Mechanical Decapsulation

<1K

                                        

Table 2. Good FA Capability

FA Equipment

Purpose

Estimated Cost (USD)

Microprobing Station

Probing / Thermography

40K - 100K

Laser Cutter

Circuit Isolation

20K - 40K

Microsectioning Equipment

Cross-sectioning

40K - 80K

High-Resolution X-ray System

X-ray Radiography

100K - 200K

Automatic Decapsulation System

Decapsulation

20K - 30K

Reactive Ion Etcher

Die Delayering

40K - 60K

SEM/EDX System

SEM / EDX Analysis

300K - 400K

                 

Table 3. Advanced FA Capability

FA Equipment

Purpose

Estimated Cost (USD)

Light Emission Microscope

Light Emission Microscopy

150K - 200K

Scanning Acoustic Microscope

Acoustic Microscopy

200K - 250K

Focused Ion Beam Machine

FIB Analysis

500K - 700K

FTIR Spectrometer

FTIR Analysis

60K - 80K

TEM System

TEM Inspection

400K - 500K

Auger Spectrometer

Auger Analysis

~1M

     

FA Techniques:   Failure Verification Optical Inspection Xray Radiography;

Curve Tracing Decapsulation Sectioning MicrothermographyLEM;

Microprobing Die Deprocessing Focused Ion Beam SEM/TEM Acoustic Microscopy;

Other FA Techniques

     

See Also:   Failure Analysis Package FailuresDie Failures Reliability Engineering;