Posted by Rivs: Tue Aug 14, 2007 8:29 am    Post subject:

 

thanks paul.  yes my hotplate temperature is 250°

as I'ved notice during decapsulation using sulfuric acid, the compound dissolves as well as the copper wire. I'ved tried to check the package from time to time.

 

Posted by Logan218142: Sat Nov 03, 2007 3:57 pm    Post subject:

 

why not try laser decap?

 

Posted by Rivs: Mon Nov 05, 2007 8:34 am    Post subject:

 

logan thanks but do you know any facility who do this?

 

Posted by Logan218142: Mon Nov 05, 2007 8:07 pm    Post subject:

 

please check website. One of them will be controlsystemation.com, which we are evaluating now. good luck.

 

Posted by Rivs: Tue Nov 06, 2007 7:56 am    Post subject:

 

logan thank you very much for this info this is really useful.

 

Posted by Paula: Mon Nov 12, 2007 12:09 pm    Post subject:

 

laser decap is on the wish list of many companies. Is anyone on the forum have this equipment? Do you have any feedback? Is it worth it?

 

Posted by Rivs: Mon Nov 12, 2007 1:06 pm    Post subject:

 

I'ved already ask everybody on the semiconductor FA I know but none of them have it, I am still searching for a facility who have this laser decap instrument

 