Table 1. Properties of some MQFP's

Part #  

No.
of Pins

Body
Size  

Body
Thickness  

Lead
Pitch  

MQFP-44 

44

10 mm x 10 mm

2 mm

0.8 mm

MQFP-52 

52

14 mm x 14 mm

2 mm

0.8 mm

MQFP-120 

120

28 mm x 28 mm

3.5 mm

0.8 mm

MQFP-208 

208

28 mm x 28 mm

3.5 mm

0.5 mm

MQFP-240 

240

32 mm x 32 mm

3.2 mm

0.5 mm

                        