MSOP - Micro Small Outline Package

                                 

 

                

The Micro Small Outline Package, or micro-SOP or MSOP, is a very small rectangular plastic package with gull wing leads protruding out of its longer sides. The MSOP is a miniaturized version of the SSOP package, having a smaller footprint than the latter.

  

 

MSOP lead counts range from 8 to 16. The typical MSOP body width is nominally 3 mm while its body thickness typically ranges from 0.85 mm to 1.1 mm. The MSOP lead pitch is typically either 0.65 mm or 0.50 mm.

      

Table 1. Properties of Some Examples of MSOP's

Part Number

No. of Pins

Body Size

Body Thickness

Lead Pitch

MSOP-8

8

2.8 mm x 2.9 mm

1.1 mm

0.65 mm

MSOP-10

10

3 mm x 3 mm

0.85 mm

0.50 mm

MSOP-12

12

3 mm x 4 mm

0.85 mm

0.65 mm

MSOP-16

16

3 mm x 4 mm

0.85 mm

0.50 mm

 

   

Figure 1.  An example of the MSOP

      