PQFP - Plastic Quad Flat Pack

                                 

 

                

The Plastic Quad Flat Pack, or PQFP, is an IC package with leads extending from all four sides of the package body. PQFP's are predominantly square in shape, although rectangular variants do exist. The PQFP is just one of the many types of the quad flat pack (QFP) package.

 

 

The PQFP comes in many body sizes, with lead counts ranging from 32 to 208. Lead pitch values used by PQFP's range from 0.4 mm to 1 mm. Typical PQFP body thickness varies from 2 mm to 3.8 mm. Lead coplanarity is very critical for PQFP's, and should be within ±4 mils for this package.

      

Table 1. Properties of some PQFP's

Part #  

No.
of Pins

Body
Size  

Body
Thick-

ness  

Lead
Pitch  

Foot-

print  

Qty
Per Tray  

Tape
Width  

Tape
Pitch

Qty
13" Reel

QFP44  

44

10mm sq  

2.0mm  

0.80mm

3.2mm  

96

24

24

500

QFP52 

52

10mm sq  

2.0mm  

0.65mm

3.2mm  

96

24

24

500

QFP52 

52

14mm sq  

2.67mm

1.00mm

3.9mm

84

32

24

350

QFP64 

64

10mm sq  

2.0mm  

0.50mm

3.2mm  

96

24

24

500

QFP64 

64

14mm sq  

2.67mm

0.80mm

3.9mm

84

32

24

350

QFP64  

64

14mm x 20mm  

2.71mm

1.00mm

3.2mm  

66

44

32

200

QFP80  

80  

14mm sq  

2.67mm  

0.65 mm

3.9mm

84

32

24

350

                        

Figure 1.  Examples of PQFP's (not in scale with each other)

      