The 'Small Outline Integrated Circuit', or SOIC, is a rectangular surface-mount integrated circuit package with eight or more gull wing leads. The leads protrude from the longer edge of the package. SOIC packages are JEDEC-compliant, and come in a variety of body widths, the most popular of which are 150 mils (narrow body) and 300 mils (wide body). The standard SOIC lead pitch is nominally 50 mils (1.27 mm).  The SOIC may be shipped in tubes or tape and reel.

 

 

The small outline package may come with J-type leads instead of gull wing leads. Such small outline packages are called 'J-Leaded Small Outline Package', or SOJ's.

                              

Table 1. Properties of some SOIC's and SOJ's

Part Number

Number
of Pins

Lead
Style

Body
Width

Qty
Per 

Tube

Tape
Width

Tape
Pitch

Qty
13" Reel

SO8G

8

Gull

3.8mm

99

12mm

8mm

2,500

SO14G

14

Gull

3.8mm

50

16mm

8mm

2,500

SO16G

16

Gull

3.8mm

50

16mm

8mm

2,500

SO16G

16

Gull

7.6mm

46

16mm

12mm

1,000

SO20G

20

Gull

7.6mm

38

24mm

12mm

1,000

SO28G

28

Gull

7.6mm

25

24mm

12mm

1,000

SO44G

44

Gull

13.3mm

17

24mm

45mm

750

SO20/26J

20/26

J-Lead

7.6mm

25

24mm

12mm

1,000

SO28J

28

J-Lead

7.6mm

27

24mm

12mm

1,000

SO32J

32

J-Lead

7.6mm

25

24mm

12mm

1,000

SO40J

40

J-Lead

10.0mm

15

44mm

16mm

500

SO42J

42

J-Lead

10.0mm

15

44mm

16mm

500

  

Figure 1.  An 8-lead SOIC (left) and a 28-lead SOJ (right)

    