Table 1.  Types of SOT Packages (not shown in scale)

Image

Name

 Typ. Lead Counts

Typ. Dimensions LxWxH (mils)

 Typ. Lead Pitch Values (mils)

SOT-23

3 to 8 115 x 63 x 40 37.5 / 50

SOT-89

3 180 x 100 x 60 120 / 60

SOT-143

4 115 x 51 x 35 75 / 65

SOT-223

4 250 x 130 x 60 180 / 90

SOT-323

 3 to 5 79 x 49 x 35 51 / 26

   