Typical UTQFN pad counts range from 6 to 28. The body thickness of UTQFN packages typically ranges from 0.50 mm to 0.60 mm. The pad pitch (distance between pads) used by UTQFN packages is usually either 0.4 mm or 0.5 mm.
Table 1. Properties of Some Examples of UTQFN's