Wedge Bonding Process Video

See more semiconductor videos

    

 

 
 

 

This is a video showing how a wire bonding machine connects the wires between the microchip and the leads going to the outside world using wedge bonds.  A wedge bond is a kind of bond that looks flat because it is produced by a wedge-shaped bonding tool,  as opposed to ball bonds which are spherical in shape and produced by another type of tool known as a capillary.

  

See also: Ball Bonding Process Video 
   

Posted in YouTube by: twloo,

 

See more semiconductor videos

 
 

Disclaimers:  The video in this page was embedded from YouTube.  This video is owned by its respective owner(s). The text description on this page was based primarily on the text description of the video on YouTube.  No copyright infringement is intended in any manner.

 